Physical Properties Metric English Comments
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
@ 23°C; ASTM F1249
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade  (discontinued **)
Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: This SBC is easily processed on blown film or cast fi..
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
@ 23°C; ASTM F1249
Chevron Phillips K-Resin® DK11 Styrene-Butadiene Copolymer, Film Grade
Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: Provides the same high performance film properties as..
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge
Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can b..
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont Teijin Films Mylar® LB Polyester Film, 75 Gauge (19 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Variet..
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont Teijin Films Mylar® LBT Polyester Film, 75 Gauge (19 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film that has been corona-treated to provide superior wetting and adhesion to inks, primers, and adhesives. Standard th..
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
Proc. E; ASTM E96
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 150 Gauge
Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a ..
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
Proc. E; ASTM E96
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 150 Gauge
Data provided by DuPont Packaging Polymers.Mylar® RL42 (formerly known as XM985) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a ..
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont Teijin Films Mylar® 50 OL Polyester Film, Ovenable Lidding, Heat Sealable, 50 Gauge
Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can b..
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont Teijin Films Mylar® HS Polyester Film, 150 Gauge (38 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe..
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
40°C, 90% RH
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ..