Polymer Property : Moisture Vapor Transmission = 1.90 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.750 cc-mm/m²-24hr-atm
1.90 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is ..
Moisture Vapor Transmission 0.750 - 1.11 cc-mm/m²-24hr-atm
1.90 - 2.82 cc-mil/100 in²-24hr-atm
40°C- 90% RH; based on 30 µm layer
Noltex Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer
Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows ..
Moisture Vapor Transmission 0.750 cc-mm/m²-24hr-atm
1.90 cc-mil/100 in²-24hr-atm
ASTM E96E-80
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film
Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc..
Moisture Vapor Transmission 0.750 cc-mm/m²-24hr-atm
1.90 cc-mil/100 in²-24hr-atm
Proc. E; ASTM E96
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 75 Gauge
Data provided by DuPont Packaging Polymers.Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film ..