Physical Properties Metric English Comments
Moisture Vapor Transmission 0.750 - 1.11 cc-mm/m²-24hr-atm
1.90 - 2.82 cc-mil/100 in²-24hr-atm
40°C- 90% RH; based on 30 µm layer
Noltex Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer
Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows ..
Moisture Vapor Transmission 0.690 - 1.11 cc-mm/m²-24hr-atm
1.75 - 2.82 cc-mil/100 in²-24hr-atm
40°C- 90% RH; based on 30 µm layer
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer
Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%...
Moisture Vapor Transmission 0.690 - 1.11 cc-mm/m²-24hr-atm
1.75 - 2.82 cc-mil/100 in²-24hr-atm
40°C- 90% RH; based on 30 µm layer
Noltex Soarnol® ET3808 Ethylene Vinyl Alcohol Copolymer
Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..