Polymer Property : Moisture Vapor Transmission = 1.93 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.760 cc-mm/m²-24hr-atm
1.93 cc-mil/100 in²-24hr-atm
ASTM E96
DuPont™ Tedlar® TUT10BG3 UV Screening Transparent Polyvinyl Fluoride Film
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o..