Material Notes:
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety of chemicals, solvents, and staining agents.Information provided by DuPont.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D1505
Moisture Absorption at Equilibrium <= 0.50 %
<= 0.50 %
ASTM D570
Moisture Vapor Transmission 0.760 cc-mm/m²-24hr-atm
1.93 cc-mil/100 in²-24hr-atm
ASTM E96
Thickness 25.4 microns
1.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD >= 95 %
>= 95 %
ASTM D882
Secant Modulus, MD 2.14 GPa
310 ksi
ASTM D822
Impact 90.3
90.3
kJ/m; Spencer; ASTM D3420
Coefficient of Friction 0.21
0.21
Film:Metal; ASTM D1894
Tear Strength 144 kN/m
822 pli
Graves (initial), MD; ASTM D1004
168 kN/m
959 pli
Graves (initial), TD; ASTM D1004
Elmendorf Tear Strength, MD 0.673 g/micron
17.1 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 0.748 g/micron
19.0 g/mil
ASTM D1922
Film Tensile Strength at Break, MD >= 89.6 MPa
>= 13000 psi
ASTM D882
Thermal Properties Metric English Comments
CTE, linear 78.0 µm/m-°C

@Temperature 50.0 - 70.0 °C
43.3 µin/in-°F

@Temperature 122 - 158 °F
MD; ASTM D696
81.0 µm/m-°C

@Temperature 50.0 - 70.0 °C
45.0 µin/in-°F

@Temperature 122 - 158 °F
TD; ASTM D696
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
DuPont 990 test
Maximum Service Temperature, Air 107 °C
225 °F
Continuous
175 °C
347 °F
Short Cycle
Minimum Service Temperature, Air -72.0 °C
-97.6 °F
Continuous
Shrinkage <= 6.0 %

@Temperature 170 °C
<= 6.0 %

@Temperature 338 °F
TD; ASTM D1204
Optical Properties Metric English Comments
Refractive Index 1.46

@Temperature 30.0 °C
1.46

@Temperature 86.0 °F
n<sub>D</sub>; Abbe Refractometer; ASTM D-542
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Aging in Air > 3000 hours to embrittlement