Polymer Property : Moisture Vapor Transmission = 48.3 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 19.0 cc-mm/m²-24hr-atm
48.3 cc-mil/100 in²-24hr-atm
ASTM F372
Eastman E6838-899F Polyethylene  (discontinued **)
E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr..