Physical Properties Metric English Comments
Carbon Dioxide Transmission 211 cc-mm/m²-24hr-atm
536 cc-mil/100 in²-24hr-atm
ASTM D1434
Eastman Tritan FX200 Copolyester
Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..