Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 47 g/10 min @Load 5.00 kg, Temperature 280 °C |
47 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |