Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 85 g/10 min @Load 5.00 kg, Temperature 265 °C |
85 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |