Polymer Property : Relative Viscosity = 1.55 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 1.55 cP
1.55 cP
QC-10-104
Formosa Plastics Formolon® 113 PVC
PVC Copolymer Suspension Resin F-113 has been developed primarily to meet the processing requirements of the vinyl composition tile (VCT) manufacturers. In addition to vinyl floor tile industry, F-1..