Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 1.85 - 1.95 cP | 1.85 - 1.95 cP | LCL-PR21 |
Intercontinental Polymers 554 PBT Polymer Type - Elastomer Polyester Pellets Applications: Engineering Resin - ModifiedInformation provided by Intercontinental Polymers. |