Polymer Property : Relative Viscosity = 1.95 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 1.85 - 1.95 cP
1.85 - 1.95 cP
LCL-PR21
Intercontinental Polymers 554 PBT Polymer Type - Elastomer Polyester Pellets
Applications: Engineering Resin - ModifiedInformation provided by Intercontinental Polymers.