Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 3.84 - 4.02 cP | 3.84 - 4.02 cP | 96% H2SO4 |
UBE 5033FDX27 Air Blown Nylon 6/66 Film Specialties: High slip typeMedium shrinkApplications: General purposeSuitable for Water cooling processProcessing: Sausage casings (Water)Big bag (Air blown)Information provided by UBE. |