Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE 5033FDX27 Air Blown Nylon 6/66 Film

Category Polymer , Film , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer UBE
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE 5033FDX27 Air Blown Nylon 6/66 Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specialties: High slip typeMedium shrinkApplications: General purposeSuitable for Water cooling processProcessing: Sausage casings (Water)Big bag (Air blown)Information provided by UBE.
Physical Properties Metric English Comments
Relative Viscosity 3.84 - 4.02 cP
3.84 - 4.02 cP
96% H2SO4
4.2 - 4.4 cP
4.2 - 4.4 cP
98% H2SO4
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 540 %
540 %
Film Elongation at Break, TD 550 %
550 %
Secant Modulus, MD 0.190 GPa
27.6 ksi
Secant Modulus, TD 0.200 GPa
29.0 ksi
Coefficient of Friction, Dynamic 0.21
0.21
Coefficient of Friction, Static 0.28
0.28
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
Film Tensile Strength at Break, TD 40.0 MPa
5800 psi
Thermal Properties Metric English Comments
Melting Point 191 - 201 °C
376 - 394 °F
Optical Properties Metric English Comments
Haze 12.4 %
12.4 %
Gloss 101 %
101 %
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F
C1
220 - 230 °C
428 - 446 °F
C2
230 - 240 °C
446 - 464 °F
C3
230 - 240 °C
446 - 464 °F
C4
240 - 250 °C
464 - 482 °F
AD
240 - 250 °C
464 - 482 °F
CF
240 - 250 °C
464 - 482 °F
D1- D4
Descriptive Properties Value Comments
Degree of Curling 9 Mm
Users viewing this material also viewed the following: