Polymer Property : Storage Temperature = 85.0 °F Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Storage Temperature 4.44 - 29.4 °C
40.0 - 85.0 °F
Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. High emissivity, inorganic black pigmented coating to 15..
Storage Temperature 4.44 - 29.4 °C
40.0 - 85.0 °F
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F.
Storage Temperature 4.44 - 29.4 °C
40.0 - 85.0 °F
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F.
Storage Temperature 4.44 - 29.4 °C
40.0 - 85.0 °F
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F.
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone
Low viscosity, green coating for power resistors to 1100°F (593°C)
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled
CP5000 is a two part, water-based, inorganic zinc rich primer which provides superior resistance to salt-fog, immersion, impact and abrasion. This primer system is compatible with all CP-Series prod..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled
Translucent-white, low-viscosity sealer for porous materials to 900°F (482°C)
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, ..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Ceramacoat™ 845-GLT High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, light-green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps,..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Ceramacoat™ 845-GRY High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, gray coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Ceramacoat™ 845-SIL High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, matte silver coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, white coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadi..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
Storage Temperature 4.44 - 29.4 °C
40.0 - 85.0 °F
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F.
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled
Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C).
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone
Low viscosity, white coating for motor windings to 1100°F (593°C)
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Storage Temperature 12.8 - 29.4 °C
55.0 - 85.0 °F
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..