Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled

Category Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Aremco
Trade Name Corr-Paint™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. High emissivity, inorganic black pigmented coating to 1500°F.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
Solids Content 46.3 %
46.3 %
by volume
50 %
50 %
by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Viscosity 600 - 900 cP
600 - 900 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
54.9 microns
2.16 mil
estimated wet film thickness
Storage Temperature 4.44 - 29.4 °C
40.0 - 85.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 816 °C
1500 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Dry Time 1.00 - 2.00 hour
1.00 - 2.00 hour
Touch
2.00 - 4.00 hour
2.00 - 4.00 hour
Handling
1 - 24 hour
1 - 24 hour
Recoat
Cure Time >= 60.0 min
>= 1.00 hour
Air Set prior to curing
120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
Curing is not required if product is exposed to a minimum of 500°F within 24-48 hours of application.
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Black
Dry Film Coverage ft2/gal 742
at 1 mil
Primer Not Required
Thinner CP3015-BL-T