Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 4.45 g/l | 4.45 g/l | |
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and .. |