Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 692 g/l | 692 g/l | ASTM D3960-89 |
Lord Adhesives Aeroglaze® Z306 Absorptive Polyurethane Aeroglaze® Z306 absorptive polyurethane coating is primarily for applications to substrates used in space operations. These operations include those where coatings must exhibit low outgassing cha.. |