Lord Adhesives Aeroglaze® Z306 Absorptive Polyurethane

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer Lord Adhesives
Trade Name Aeroglaze®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Aeroglaze® Z306 Absorptive Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aeroglaze® Z306 absorptive polyurethane coating is primarily for applications to substrates used in space operations. These operations include those where coatings must exhibit low outgassing characteristics while providing high thermal absorptivity properties.In addition, the mechanical properties required for rigorous durations in space are an integral part of the Aeroglaze Z306 absorptive polyurethane make-up. Aeroglaze Z306 absorptive polyurethane shows excellent performance on rigid or flexible substrates.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D1475-85
Solids Content 23 %
23 %
by volume
27 %
27 %
by weight
Volatile Organic Compounds (VOC) Content 692 g/l
692 g/l
ASTM D3960-89
Brookfield Viscosity 60 cP

@Temperature 25.0 °C
60 cP

@Temperature 77.0 °F
ASTM D2196-86; LVT
Outgassing - Total Mass Loss 1.0 %
1.0 %
ASTM E595-77
Thermal Properties Metric English Comments
Flash Point 19.0 °C
66.2 °F
Setaflash, Closed Cup; ASTM D3278-82
Optical Properties Metric English Comments
Gloss <= 10 %
<= 10 %
85°
Emissivity (0-1) 0.90
0.90
ASTM E408-71
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 25.0 °C
2.00 - 3.00 hour

@Temperature 77.0 °F
Tack Free; 50% relative humidity
720 min

@Temperature 25.0 °C
12.0 hour

@Temperature 77.0 °F
Permit Handling
2160 - 2880 min

@Temperature 25.0 °C
36.0 - 48.0 hour

@Temperature 77.0 °F
Permit Normal Usage
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Flat Black
Solar Absorption >0.95
Gier-Dunkle Integrating Sphere
Theoretical Coverage (ft²/gallon/mil) 368