Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 87.7 g/l
87.7 g/l
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive
TRA-BOND 2119 is a crystal clear adhesive specifically designed for bonding glass to glass and glass to plastics. It also yields a high lap shear strength to metals and ceramics. This system cures t..