Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.918 - 0.923 g/cc @Temperature 23.0 °C |
0.0332 - 0.0333 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT 17-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.920 - 0.925 g/cc @Temperature 20.0 °C |
0.0332 - 0.0334 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE2NT 17-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.918 - 0.923 g/cc @Temperature 23.0 °C |
0.0332 - 0.0333 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT 18-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.920 - 0.925 g/cc @Temperature 20.0 °C |
0.0332 - 0.0334 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE2NT 18-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.918 - 0.923 g/cc @Temperature 23.0 °C |
0.0332 - 0.0333 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT 15-10 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.920 - 0.925 g/cc @Temperature 20.0 °C |
0.0332 - 0.0334 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE2NT 15-10 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.918 - 0.923 g/cc @Temperature 23.0 °C |
0.0332 - 0.0333 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT 15-5 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.920 - 0.925 g/cc @Temperature 20.0 °C |
0.0332 - 0.0334 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE2NT 15-5 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.918 - 0.923 g/cc @Temperature 23.0 °C |
0.0332 - 0.0333 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT 16-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.920 - 0.925 g/cc @Temperature 20.0 °C |
0.0332 - 0.0334 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE2NT 16-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.918 - 0.923 g/cc @Temperature 23.0 °C |
0.0332 - 0.0333 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT 17-5 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Density | 0.920 - 0.925 g/cc @Temperature 20.0 °C |
0.0332 - 0.0334 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE2NT 17-5 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |