Kazanorgsintez PE2NT 17-5 Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez PE2NT 17-5 Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 0.918 - 0.923 g/cc

@Temperature 23.0 °C
0.0332 - 0.0333 lb/in³

@Temperature 73.4 °F
0.920 - 0.925 g/cc

@Temperature 20.0 °C
0.0332 - 0.0334 lb/in³

@Temperature 68.0 °F
Melt Flow 1.5 - 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 - 2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
±10%
30 - 84 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30 - 84 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 9.00 MPa
>= 1310 psi
Elongation at Break >= 700 %
>= 700 %
Tear Strength Test >= 20
>= 20
MPa
Descriptive Properties Value Comments
Amount of impurities [pcs] 8
Users viewing this material also viewed the following: