Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.958 - 0.965 g/cc @Temperature 23.0 °C |
0.0346 - 0.0349 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT22-12 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Density | 0.960 - 0.966 g/cc @Temperature 20.0 °C |
0.0347 - 0.0349 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE2NT22-12 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |