Physical Properties Metric English Comments
Density 0.960 - 0.966 g/cc

@Temperature 20.0 °C
0.0347 - 0.0349 lb/in³

@Temperature 68.0 °F
Kazanorgsintez PE2NT22-12 High Density Polyethylene Composite
Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin..