Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 3550 cSt @Temperature 37.8 °C |
3550 cSt @Temperature 100 °F |
ASTM D445-94 |
Dow VORANOL™ RA 800 Polyol VORANOL™ RA 800 polyol is a highly reactive amine initiated polyether polyol, specially developed for the production of rigid polyurethane foams and designed for blending with other polyols.Informa.. |