Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.0011 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QCL349 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, Flame Retardant, Elect..
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized...
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 (Asia Pacific)
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC
LNP THERMOCOMP* DF006ER is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11
LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.0011 - 0.0016 cm/cm

@Time 86400 sec
0.0011 - 0.0016 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12
LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0011 - 0.0016 cm/cm

@Time 86400 sec
0.0011 - 0.0016 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK
LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am..
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66
LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0011 - 0.0016 cm/cm

@Time 86400 sec
0.0011 - 0.0016 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas ..
Linear Mold Shrinkage, Flow 0.0011 - 0.0030 cm/cm

@Time 86400 sec
0.0011 - 0.0030 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6
LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Verton NV006E PC/ABS
LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas region..
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON NV006E PC/ABS (Asia Pacific)
LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10
LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti..
Linear Mold Shrinkage, Flow 0.0011 cm/cm

@Time 86400 sec
0.0011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON NV006E PC+ABS
LNP* Verton* NV006E is a compound based on PC+ABS blend resin containing 30% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.
Copyright © lookpolymers.com All Rights Reserved