Polymer Property : Linear Mold Shrinkage, Flow = 0.0033 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC
LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by ..
Linear Mold Shrinkage, Flow 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI (Asia Pacific)
LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RVL28 PA 66
LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura..
Linear Mold Shrinkage, Flow 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC
LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI
LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable.