Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 732 °C | 1350 °F | Ac1 |
Latrobe LSSâ„¢ 4140 Alloy Steel (AISI 4140) TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co.. |
|||
Critical Temperature | 732 °C | 1350 °F | Ac1 |
Latrobe LSSâ„¢ 4142 Alloy Steel (AISI 4142) TLS 4140 and 4142HT are versatile, alloy steels which are used in variety of tooling and other industrial applications. TLS 4140 is the classic AISI 4140 alloy steel which is sold in the annealed co.. |
|||
Critical Temperature | 730 °C | 1350 °F | Ar1 |
Latrobe CM-50â„¢ ASTM M50 High Speed Steel CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking to.. |
|||
Critical Temperature | 732 °C | 1350 °F | Ac1 |
Latrobe LSSâ„¢ 2714 Hot Work Tool Steel (DIN 1.2714 mod) TLS 2714 is a nickel-chromium-molybdenum hot work steel that exhibits high impact toughness and good resistance to softening at elevated temperature. The high nickel content imparts the toughness as.. |
|||
Critical Temperature | 732 °C | 1350 °F | Ac1 |
Latrobe LSSâ„¢ 2714T Hot Work Tool Steel (DIN 1.2714 mod) TLS 2714HT is the same steel available from inventory in a heat-treated condition, at a hardness of 352 to 401 HBS (approximately 38 to 43 HRC). TLS 2714HT can be readily flame cut, and this propert.. |
|||
Critical Temperature | 732 °C | 1350 °F | Ar3 |
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11) TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides.. |
|||
Critical Temperature | 732 °C | 1350 °F | Ac1 |
Latrobe LSS™ O1 Tool Steel (ASTM O1) TLS O1 tool steel is the original oil-hardening, "non-shrinking" tool steel that can be hardened to the Rockwell C 65 range from a low austenitizing temperature. TLS O1 is a general-purpose tool ste.. |
|||
Critical Temperature | 730 °C | 1350 °F | Ar3 |
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1) TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load.. |