Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 788 °C | 1450 °F | Ac1 |
Latrobe LSSâ„¢ D2 Tool Steel (ASTM D2) TLS D2 tool steel is a versatile high-carbon, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium rich alloy carbides.. |
|||
Critical Temperature | 789 °C | 1450 °F | Ar1 |
Latrobe LSSâ„¢ D2 Tool Steel (ASTM D2) TLS D2 tool steel is a versatile high-carbon, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium rich alloy carbides.. |
|||
Critical Temperature | 785 °C | 1450 °F | Ar1 |
Latrobe DuraTechâ„¢ T15 Powder Metal High Speed Steel (ASTM T15) DuraTech T15 powder metallurgy high speed steel is cobalt-bearing super high speed steel which can be heat treated to a hardness as high as 67 Rockwell C. A high volume of hard vanadium carbides pro.. |
|||
Critical Temperature | 785 °C | 1450 °F | Ar1 |
Latrobe Dynavanâ„¢ ASTM T15 Super High Speed Steel DYNAVAN (T15) is a super high speed steel designed for extra-high wear resistance and superior hot hardness. These properties result from the high carbon and vanadium contents which produce numerous.. |