Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe LSSâ„¢ D2 Tool Steel (ASTM D2)

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel , Tool Steel , Air-Hardening Steel
Manufacturer Latrobe Steel
Trade Name LSS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSSâ„¢ D2 Tool Steel (ASTM D2).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TLS D2 tool steel is a versatile high-carbon, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium rich alloy carbides in the microstructure. These carbides provide good resistance to wear from sliding contact with other metals and abrasive materials. Although other steels with improved toughness or improved wear resistance are available, TLS D2 provides an effective combination of wear resistance and toughness, tool performance, price, and a wide variety of product forms. TLS D2 is also available as an Electro-Slag-Remelted (ESR) product. The remelting process provides improved chemical homogeneity, refinement of carbide size, and the associated improvements in mechanical and fatigue properties. Typical applications for TLS D2 tool steel include rolls, punches, dies for blanking, forming, trimming, and thread rolling, shear knives, food-processing knives, and gages.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.70 g/cc
7.70 g/cc
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 62.5
62.5
Air Cooled from 982°C, 30 minutes
63
63
Air Cooled from 1038°C, 30 minutes
64
64
Air Cooled from 1010°C, 30 minutes
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 50 - 60 %
50 - 60 %
1% Carbon Steel
Izod Impact Unnotched 10.8 J
8.00 ft-lb
Air Cooled from 1010°C; As Quenched
29.8 J
22.0 ft-lb
Air Cooled from 1010°C; 483°C Temper Temperature
55.6 J
41.0 ft-lb
Air Cooled from 1010°C; 593°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 10.3 µm/m-°C

@Temperature 38.0 - 260 °C
5.72 µin/in-°F

@Temperature 100 - 500 °F
12.3 µm/m-°C

@Temperature 38.0 - 538 °C
6.83 µin/in-°F

@Temperature 100 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 1.5 %
1.5 %
Chromium, Cr 12 %
12 %
Iron, Fe 85.6 %
85.6 %
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 0.75 %
0.75 %
Silicon, Si 0.30 %
0.30 %
Vanadium, V 0.90 %
0.90 %
Chemical Properties Metric English Comments
Critical Temperature 744 °C
1370 °F
Ar3
788 °C
1450 °F
Ac1
789 °C
1450 °F
Ar1
1553 °C
2827 °F
Ac3
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved