Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 336 °C | 637 °F | Martensitic Start |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 17 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Critical Temperature | 336 °C | 637 °F | Martensitic Start |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 9 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Critical Temperature | 336 °C | 637 °F | Martensitic Start |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 13.5 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Critical Temperature | 336 °C | 637 °F | Martensitic Start |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 6 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |