Chemical Properties Metric English Comments
Critical Temperature 760 °C
1400 °F
Ar1
Latrobe Tatmoâ„¢ ASTM M1 High Speed Steel
TATMO is an M1-type, general-purpose high speed steel. In comparison with other popular high speed steels, it exhibits excellent toughness and grindability. These factors and its relatively low cost..
Critical Temperature 760 °C
1400 °F
Ac3
Latrobe LSS™ O1 Tool Steel (ASTM O1)
TLS O1 tool steel is the original oil-hardening, "non-shrinking" tool steel that can be hardened to the Rockwell C 65 range from a low austenitizing temperature. TLS O1 is a general-purpose tool ste..