Material Notes:
TATMO is an M1-type, general-purpose high speed steel. In comparison with other popular high speed steels, it exhibits excellent toughness and grindability. These factors and its relatively low cost make it an economic and efficient tool material. Typical applications for Tatmo high speed steel include twist drills, taps, milling cutters, reamers, broaches, saws, and knives.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.89 g/cc
7.89 g/cc
Density 7.89 g/cc
0.285 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 64.5
64.5
Oil Quenched from 1232°C
65.5
65.5
Oil Quenched from 1121°C
66.5
66.5
Oil Quenched from 1177°C
Modulus of Elasticity 214 GPa
31000 ksi
Machinability 55 - 65 %
55 - 65 %
1% Carbon Steel
Izod Impact Unnotched 38.0 J
28.0 ft-lb
Oil Quenched at 1218°C; 482°C Temper Temperature
44.7 J
33.0 ft-lb
Oil Quenched at 1218°C; 622°C Temper Temperature
51.5 J
38.0 ft-lb
Oil Quenched at 1218°C; 580°C Temper Temperature
71.9 J
53.0 ft-lb
Oil Quenched at 1163°C; 482°C Temper Temperature
77.3 J
57.0 ft-lb
Oil Quenched at 1163°C; 622°C Temper Temperature
90.8 J
67.0 ft-lb
Oil Quenched at 1163°C; 580°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 10.07 µm/m-°C

@Temperature 38.0 - 260 °C
5.594 µin/in-°F

@Temperature 100 - 500 °F
12.33 µm/m-°C

@Temperature 38.0 - 649 °C
6.850 µin/in-°F

@Temperature 100 - 1200 °F
Component Elements Properties Metric English Comments
Carbon, C 0.83 %
0.83 %
Chromium, Cr 3.75 %
3.75 %
Iron, Fe 83.47 %
83.47 %
Manganese, Mn 0.25 %
0.25 %
Molybdenum, Mo 8.5 %
8.5 %
Silicon, Si 0.30 %
0.30 %
Tungsten, W 1.75 %
1.75 %
Vanadium, V 1.15 %
1.15 %
Chemical Properties Metric English Comments
Critical Temperature 724 °C
1340 °F
Ar3
760 °C
1400 °F
Ar1
827 °C
1520 °F
Ac1
860 °C
1580 °F
Ac3