Polymer Property : Ionic Impurities - Na (Sodium) = 10 ppm Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Ionic Impurities - Na (Sodium) <= 10 ppm
<= 10 ppm
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant
TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low..
Ionic Impurities - Na (Sodium) 10 ppm
10 ppm
Tra-Con Tra-Bond 7560D Hydrolytically Stable Adhesive
TRA-BOND 7560D is an electrically insulating epoxy adhesive. This material has a 10 day work life and a medium viscosity for easy usage. There are also multiple cure options that make this product i..
Ionic Impurities - Na (Sodium) 10 ppm
10 ppm
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy
Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as..
Ionic Impurities - Na (Sodium) 10 ppm
10 ppm
Epoxy Technology EPO-TEK® E2101 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E2101 is a two component, thixotropic, electrically conductive adhesive. It may be used for circuit assembly and semiconductor applications. Advantages & Application ..
Ionic Impurities - Na (Sodium) <= 10 ppm
<= 10 ppm
AOD-S
Dow VORANOL™ CP 755 Polyol
VORANOL™ CP 755 polyol is a glycerine propoxylated polyether triol.Information provided by Dow
Ionic Impurities - Na (Sodium) <= 10 ppm
<= 10 ppm
AOD-S
Dow VORANOL™ CP 450 Polyol
VORANOL™ CP 450 polyol is a glycerine propoxylated polyether triol.Information provided by Dow