Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K Factor (ISO) 4.0 µm/km
4.0 µm/km
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data)
TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa..
K Factor (ISO) 4.0 µm/km
4.0 µm/km
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data)
TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain..