Polymer Property : Tensile Impact = 128 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact 68.3 - 131 J/cm
128 - 245 ft-lb/in
Average value: 110 J/cm Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
Tensile Impact 68.3 J/cm
128 ft-lb/in
ASTM D1822
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Blow Molding Grade)
ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac..
Tensile Impact 68.3 J/cm
128 ft-lb/in
ASTM D1822
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Sheet & Profile Grade)
ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Regulatory StatusThe base resin LR 7320 meets t..
Tensile Impact 68.3 J/cm
128 ft-lb/in
ASTM D1822
LyondellBasell Petrothene® LR732011 High Density Polyethylene (Blow Molding Grade)
ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac..
Tensile Impact 68.3 J/cm
128 ft-lb/in
ASTM D1822
LyondellBasell Petrothene® LR732013 High Density Polyethylene (Blow Molding Grade)
ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac..
Tensile Impact 68.3 J/cm
128 ft-lb/in
ASTM D1822
LyondellBasell Petrothene® LR732031 High Density Polyethylene
ApplicationsPETROTHENE LR 7320-31 is a high density polyethylene resin that exhibits an excellent balance of stiffness and environmental stress crack resistance. This resin has outstanding extrusio..
Tensile Impact 68.3 - 152 J/cm
128 - 285 ft-lb/in
Average value: 88.4 J/cm Grade Count:6
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..