Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.937 - 1.06 g/cc
0.0339 - 0.0383 lb/in³
Average value: 0.957 g/cc Grade Count:19
Environmental Stress Crack Resistance 30.0 - 1500 hour
30.0 - 1500 hour
Average value: 671 hour Grade Count:9
Melt Flow 0.200 - 21.0 g/10 min
0.200 - 21.0 g/10 min
Average value: 5.24 g/10 min Grade Count:13
Mechanical Properties Metric English Comments
Hardness, Rockwell R 60.0 - 70.0
60.0 - 70.0
Average value: 65.0 Grade Count:4
Hardness, Shore D 65.0 - 67.0
65.0 - 67.0
Average value: 65.9 Grade Count:7
Tensile Strength, Ultimate 21.4 - 30.3 MPa
3100 - 4390 psi
Average value: 26.2 MPa Grade Count:5
Tensile Strength, Yield 17.9 - 31.0 MPa
2600 - 4500 psi
Average value: 25.9 MPa Grade Count:15
Elongation at Break 500 - 800 %
500 - 800 %
Average value: 654 % Grade Count:13
Flexural Yield Strength 22.8 - 37.9 MPa
3310 - 5500 psi
Average value: 29.8 MPa Grade Count:5
Flexural Modulus 0.779 - 1.55 GPa
113 - 225 ksi
Average value: 1.18 GPa Grade Count:18
Izod Impact, Notched 5.30 - 7.50 J/cm
9.93 - 14.1 ft-lb/in
Average value: 6.57 J/cm Grade Count:3
4.30 - 5.30 J/cm

@Temperature -29.0 - -29.0 °C
8.06 - 9.93 ft-lb/in

@Temperature -20.2 - -20.2 °F
Average value: 4.63 J/cm Grade Count:3
Gardner Impact 34.0 - 36.0 J
25.1 - 26.6 ft-lb
Average value: 34.5 J Grade Count:4
Tensile Impact 68.3 - 131 J/cm
128 - 245 ft-lb/in
Average value: 110 J/cm Grade Count:3
Falling Dart Impact 271.164 - 271.164 J

@Temperature -40.0 - -40.0 °C
200.000 - 200.000 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 271 J Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 108 - 120 µm/m-°C
60.0 - 66.7 µin/in-°F
Average value: 116 µm/m-°C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 57.0 - 92.0 °C
135 - 198 °F
Average value: 74.1 °C Grade Count:10
Vicat Softening Point 122 - 134 °C
252 - 273 °F
Average value: 127 °C Grade Count:5
Brittleness Temperature -118 - -75.0 °C
-180 - -103 °F
Average value: -87.7 °C Grade Count:9