Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 102 N | 22.9 lb (f) | PPT Tear Resistance, MD; ASTM D2582 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Tear Strength, Total | 102 N | 22.9 lb (f) | PPT Tear Resistance, MD; ASTM D2582 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |