Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength, Total = 22.9 lb (f) Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength, Total 102 N
22.9 lb (f)
PPT Tear Resistance, MD; ASTM D2582
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Tear Strength, Total 102 N
22.9 lb (f)
PPT Tear Resistance, MD; ASTM D2582
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Copyright © lookpolymers.com All Rights Reserved