Polymer Property : Tear Strength, Total = 21.0 N Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength, Total 21.0 N
4.72 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® 411 Paper, 15 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Tear Strength, Total 21.0 N
4.72 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® 411 Paper, 23 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Tear Strength, Total 21.0 N
4.72 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Copyright © lookpolymers.com All Rights Reserved