Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 21.0 N | 4.72 lb (f) | Initial in MD; ASTM D1004 |
DuPont™ Nomex® 411 Paper, 15 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Tear Strength, Total | 21.0 N | 4.72 lb (f) | Initial in TD; ASTM D1004 |
DuPont™ Nomex® 411 Paper, 23 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Tear Strength, Total | 21.0 N | 4.72 lb (f) | Initial in TD; ASTM D1004 |
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |