Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 2230 N | 501 lb (f) | TD, Graves; ASTM D1004 |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |