Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 3290 N | 740 lb (f) | Graves, TD; ASTM D1004 |
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E.. |