Mechanical Properties Metric English Comments
Tensile Strength 0.0724 MPa
10.5 psi
ASTM D412
Rogers Corporation Bisco® MF1 8055 - 55 Silicone, High Performance Foam, Indentation Force Material
MF1® 8055 is a high quality silicone foam material designed for a wide range of cushioning and sealing applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superi..