Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Rogers Corporation Bisco® MF1 8055 - 55 Silicone, High Performance Foam, Indentation Force Material

Category Polymer , Thermoset , Silicone , Silicone Foam
Manufacturer Rogers Corporation
Trade Name Bisco®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rogers Corporation Bisco® MF1 8055 - 55 Silicone, High Performance Foam, Indentation Force Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MF1® 8055 is a high quality silicone foam material designed for a wide range of cushioning and sealing applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superior weather- and UV-resistance, and low compression set to endure safety, long-term comfort and durability. White is the standard color for MF1 foam. Available as slab or to specification.Information provided by Rogers Corporation.
Physical Properties Metric English Comments
Density 0.128 g/cc
0.00463 lb/in³
ASTM D1056
Mechanical Properties Metric English Comments
Tensile Strength 0.0724 MPa
10.5 psi
ASTM D412
Elongation at Break >= 60 %
>= 60 %
ASTM D412
Compression Set 0.00 %

@Temperature 70.0 °C,
Time 79200 sec
0.00 %

@Temperature 158 °F,
Time 22.0 hour
50% compressed % max; ASTM D1056
0.00 %

@Temperature 100 °C,
Time 79200 sec
0.00 %

@Temperature 212 °F,
Time 22.0 hour
50% compressed % max; ASTM D1056
Thermal Properties Metric English Comments
Flame Spread Index <= 25
<= 25
BS 6853 - cat 1a (composite); BS 5852 - crib 7 (composite); PrEN 45545 - HL4; ASTM E162/ D3675
Smoke Density 1.5 min
1.5 min
<50; ASTM E662
4.0 min
4.0 min
<20; ASTM E662
Descriptive Properties Value Comments
Durability 0% height loss
Jounce & Squim (1,000,000 cycles)
Flammability Test Pass
FAR 25.853 (a)(1)(i); 60 sec
Pass
FAR 25.853 (a)(1)(i); 12 sec
Indentation Force Deflection 55 lbs
ASTM D3574 B1; @ 2" thick
Toxic Gas Emissions Pass
Bombardier SMP 800C