Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.740 MPa | 107 psi | ISO 7214 1998 |
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Tensile Strength | 0.740 MPa | 107 psi | DIN EN ISO 1798 |
BASF Neopolen® P 8225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Tensile Strength | 0.740 MPa | 107 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9035 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Tensile Strength | 0.740 MPa | 107 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Tensile Strength | 0.740 MPa | 107 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9230 D 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Tensile Strength | 0.740 MPa | 107 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9230 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Tensile Strength | 0.740 MPa | 107 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9335 MG 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Tensile Strength | 0.740 MPa | 107 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9435 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Tensile Strength | 0.740 MPa | 107 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9230 A 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Tensile Strength | 0.740 MPa | 107 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9235 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |