Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.411 MPa | 204.6 psi | ISO 1798 |
Zotefoams ZOTEK® F 74 HT PVDF Foam Zotek® F 74 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |