Mechanical Properties Metric English Comments
Tensile Strength >= 10.69 MPa
>= 1551 psi
ASTM D412 Method A
Seals Eastern 7042U Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..