Material Notes:
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type 1 (Viton A)Excellent mechanical propertiesGood extrusion resistanceChemical and heat resistantViton® is a registered trademark of DuPont. Information provided by Seals Eastern.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 84
>= 84
ASTM D2240
88
88
Average; ASTM D2240
Tensile Strength >= 10.69 MPa
>= 1551 psi
ASTM D412 Method A
14.84 MPa
2153 psi
Average; ASTM D412 Method A
Tensile Stress >= 1.37 MPa

@Strain 100 %
>= 199 psi

@Strain 100 %
ASTM D412 Method A
>= 3.61 MPa

@Strain 50.0 %
>= 524 psi

@Strain 50.0 %
ASTM D412 Method A
4.16 MPa

@Strain 25.0 %
603 psi

@Strain 25.0 %
Average; ASTM D412 Method A
6.14 MPa

@Strain 50.0 %
891 psi

@Strain 50.0 %
Average; ASTM D412 Method A
9.556 MPa

@Strain 100 %
1386 psi

@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 71 %
>= 71 %
ASTM D412 Method A
151 %
151 %
Average; ASTM D412 Method A
Tear Strength Test 304
304
psi; ASTM D624, Die B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy/ Unit Volume at 20% Elongation (psi) 69
ASTM D412 Method A