Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 101 MPa | 14700 psi | ASTM D638 |
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
Tensile Strength | 101 MPa | 14600 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan.. |
|||
Tensile Strength | 101 MPa | 14700 psi | Machine; IPC TM-650 2.4.18.3 |
Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System MULTICLAD™ HF represents the next generation low-loss thermoset and prepreg system for high-speed and high-frequency printed circuit boards. This technology combines a low-loss, high reliability t.. |
|||
Tensile Strength | 101 MPa | 14700 psi | ASTM D638 |
Aaron Industries AAROPRENE® GFABS 4040 Glass Filled Acrylonitrile-Butadiene Styrene AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |